Back to Search Start Over

Degradability of Polyurethanes and Their Blends with Polylactide, Chitosan and Starch

Authors :
Ingeniería química y del medio ambiente
Ingeniaritza kimikoa eta ingurumenaren ingeniaritza
Brzeska, Joanna
Tercjak Sliwinska, Agnieszka
Sikorska, Wanda
Mendrek, Barbara
Kowalczuk, Marek
Rutkowska, Maria
Ingeniería química y del medio ambiente
Ingeniaritza kimikoa eta ingurumenaren ingeniaritza
Brzeska, Joanna
Tercjak Sliwinska, Agnieszka
Sikorska, Wanda
Mendrek, Barbara
Kowalczuk, Marek
Rutkowska, Maria
Publication Year :
2021

Abstract

One of the methods of making traditional polymers more environmentally friendly is to modify them with natural materials or their biodegradable, synthetic equivalents. It was assumed that blends with polylactide (PLA), polysaccharides: chitosan (Ch) and starch (St) of branched polyurethane (PUR) based on synthetic poly([R,S]-3-hydroxybutyrate) (R,S-PHB) would degrade faster in the processes of hydrolysis and oxidation than pure PUR. For the sake of simplicity in the publication, all three modifiers: commercial PLA, Ch created by chemical modification of chitin and St are called bioadditives. The samples were incubated in a hydrolytic and oxidizing environment for 36 weeks and 11 weeks, respectively. The degradation process was assessed by observation of the chemical structure as well as the change in the mass of the samples, their molecular weight, surface morphology and thermal properties. It was found that the PUR samples with the highest amount of R,S-PHB and the lowest amount of polycaprolactone triol (PCLtriol) were degraded the most. Moreover, blending with St had the greatest impact on the susceptibility to degradation of PUR. However, the rate of weight loss of the samples was low, and after 36 weeks of incubation in the hydrolytic solution, it did not exceed 7% by weight. The weight loss of Ch and PLA blends was even smaller. However, a significant reduction in molecular weight, changes in morphology and changes in thermal properties indicated that the degradation of the samples should occur quickly after this time. Therefore, when using these polyurethanes and their blends, it should be taken into account that they should decompose slowly in their initial life. In summary, this process can be modified by changing the amount of R,S-PHB, the degree of cross-linking, and the type and amount of second blend component added (bioadditives).

Details

Database :
OAIster
Notes :
This research was founded by the National Science Center Poland Miniatura 2 project no. 2018/02/X/ST5/02005 and partially by the UMG research project no. WZNJ/2021/PZ/02., English
Publication Type :
Electronic Resource
Accession number :
edsoai.on1256624097
Document Type :
Electronic Resource