Back to Search Start Over

Environmental effects on graphite fiber reinforced PMR-15 polyimide

Authors :
Serafini, T. T
Hanson, M. P
Publication Year :
1980
Publisher :
United States: NASA Center for Aerospace Information (CASI), 1980.

Abstract

Studies were conducted to establish the effects of thermo-oxidative and hydrothermal exposure on the mechanical properties of T300 graphite fabric reinforced PMR-15 composites. The effects of hydrothermal exposure on the mechanical properties of HTS-2 continuous graphite fiber composites were also investigated. The thermo-oxidative stability characteristics of T300 fabric and T300 fabric/PMR-15 composites were determined. Flexural strengths of specimens were determined. The useful lifetime of T300 fabric/PMR-15 composites in air at 316 C was found to be about 100 hours. The useful lifetimes in air at 228 and 260 C were determined to be 500 and 1000 hours, respectively. Absorbed moisture was found to reduce the elevated temperature properties of both the T300 fabricate and HTS-2 continuous fiber composites. The moisture effect was found to be reversible.

Subjects

Subjects :
Composite Materials

Details

Language :
English
Database :
NASA Technical Reports
Notes :
RTOP 505-33-32
Publication Type :
Report
Accession number :
edsnas.19810023651
Document Type :
Report