- Hot press butt welds were made in 0.5 in. diameter bar, and roll lap welds were made in 0.060 in. thick sheet of Ti-6A1-4V. For hot press welds made after auto-vacuum cleaning at 1800 F for 2 hours, weld strength and ductility equaled the parent metal properties. Only 5 minutes of pressing time were needed at 1800 F and 200 psi to make the hot press welds. Roll welds were made in sheet at 1750 F with only 10 percent deformation. The welds in the bar and sheet were metallurgically indistinguishable from the parent material.
- Subjects :
- Materials, Metallic
Subjects
Details
- Language :
- English
- Database :
- NASA Technical Reports
- Notes :
- RTOP 114-03
- Publication Type :
- Report
- Accession number :
- edsnas.19720023902
- Document Type :
- Report