Processing and Characterization of Spark Plasma Sintered SiC-TiB2-TiC Powders

Authors :
Sergey N. Grigoriev
Yuri Pristinskiy
Thet Naing Soe
Alexander Malakhinsky
Mikhail Mosyanov
Pavel Podrabinnik
Anton Smirnov
Nestor Washington Solís Pinargote
Source :
Materials, Vol 15, Iss 5, p 1946 (2022)
Publication Year :
2022
Publisher :
MDPI AG, 2022.

Abstract

SiC-TiB2-TiC composites with matrices consisting of semiconductor material (SiC), conductive materials (TiB2-TiC), or their combination were fabricated by spark plasma sintering (SPS) at 2000 °C in a vacuum under a pressure of 80 MPa for 3 min. The composition and microstructure of the obtained composites were studied by X-ray diffraction and a scanning electron microscope equipped with an energy-dispersive detector. The flexural strength, Vickers hardness, and fracture toughness of SPSed samples were determined. Based on the observations in this work, three variations of the sintering process were proposed with different matrix compositions. The dense (99.7%) 60SiC-25TiB2-15TiC vol.% sintered ceramic composites exhibited the highest strength and hardness values of the studied composites, as well as a fracture toughness of 6.2 MPa·m1/2.

Details

Language :
English
ISSN :
19961944
Volume :
15
Issue :
5
Database :
Directory of Open Access Journals
Journal :
Materials
Publication Type :
Academic Journal
Accession number :
edsdoj.8781d846de3546b58dd27b330368d30a
Document Type :
article
Full Text :
https://doi.org/10.3390/ma15051946