Abstract

While the use of low-melting-point metals as sintering aids for high-entropy carbide (HEC) ceramics has been well established, their existence can compromise hardness due to residual metallic inclusions. This study demonstrates an innovative strategy to meet this challenge, where (Ti,Zr,Nb,Ta,Mo)C high-entropy carbide ceramics with ultrafine grains and enhanced hardness are obtained through chromium (Cr)-metal-assisted spark plasma sintering (SPS) at a temperature as low as 1600 °C. The results show that the addition of 5 vol% Cr promotes the formation of highly densified single HEC phase ceramics with a high relative density (98.4%) and an ultrafine-grained microstructure (0.17 μm). This low-temperature densification mechanism can be attributed to Cr’s solid-solution effect within the matrix and the increased carbon vacancies generated during sintering. The grain size of the (Ti,Zr,Nb,Ta,Mo)C ceramics with 5 vol% Cr metal addition is significantly smaller than that of Cr-free (Ti,Zr,Nb,Ta,Mo)C ceramics sintered at 2000 °C (3.03 μm) or via traditional low-temperature liquid-phase sintering (1.3–1.5 μm). Importantly, the addition of 5 vol% Cr substantially increased the hardness of the ceramics, with a remarkable increase from 23.57 to 28.16 GPa compared to that of the pure (Ti,Zr,Nb,Ta,Mo)C ceramics, owing to the fine-grain strengthening and solid-solution strengthening mechanisms. This work highlights the uniqueness of Cr metal as a sintering aid in achieving densification and hardness improvements in (Ti,Zr,Nb,Ta,Mo)C ceramics, offering a promising strategy for improving the properties of HEC materials for further development in the near future.

Details

Language :
English
ISSN :
22264108 and 22278508
Volume :
13
Issue :
6
Database :
Directory of Open Access Journals
Journal :
Journal of Advanced Ceramics
Publication Type :
Academic Journal
Accession number :
edsdoj.6f116fd577b34dd6a7af4c3baa7c63aa
Document Type :
article
Full Text :
https://doi.org/10.26599/JAC.2024.9220896