Wear Behaviour of Polymer-Infiltrated Network Ceramics, Lithium Disilicate and Cubic Zirconia against Enamel in a Bruxism-Simulated Scenario
- Source :
- Biomedicines, Vol 10, Iss 7, p 1682 (2022)
- Publication Year :
- 2022
- Publisher :
- MDPI AG, 2022.
-
Abstract
- The present study aimed to evaluate the wear rate of polymer-infiltrated network composites and ceramics against enamel in a bruxism-simulated scenario. Ninety-six (n = 96) molars were divided into six groups (n = 16) according to their occlusal material: group 1—a polymer-infiltrated network ceramic (PINC); group 2—a second polymer-infiltrated network ceramic (PINC2); group 3—nanohybrid resin-based composite (CO); group 4—cubic zirconia (ZR); group 5—lithium disilicate (LS); and group 6—sound enamel (EN). A laser scanner was used to digitalize all of the occlusal surfaces before and after a fatigue test, which was conducted with a chewing simulator set at 80 N and semicircular movement in order to simulate bruxist movement and loads. Statistical analysis of volume loss was performed with a one-way ANOVA and post hoc Bonferroni test. ZR had significantly inferior wear to PINC (p ≤ 0.01) and CO (p = 0.04). LS wore the antagonist enamel significantly more than PINC, CO, PINC2 and EN (p ≤ 0.01). On the other hand, ZR wore the antagonist enamel significantly more than CO (p ≤ 0.01) and PINC2 (p = 0.05). In conclusion, PINCs better preserved antagonist enamel at the expense of a higher wear of their own. LS causes significantly higher enamel wear compared with PINCs. ZR caused significantly higher enamel wear compared with CO and PINC2, but it was wear-resistant.
Details
- Language :
- English
- ISSN :
- 22279059
- Volume :
- 10
- Issue :
- 7
- Database :
- Directory of Open Access Journals
- Journal :
- Biomedicines
- Publication Type :
- Academic Journal
- Accession number :
- edsdoj.0d94b1abd4ddeaa06210bb82f1004
- Document Type :
- article
- Full Text :
- https://doi.org/10.3390/biomedicines10071682