Impact of the Top SiO2 Interlayer Thickness on Memory Window of Si Channel FeFET with TiN/SiO2/Hf0.5Zr0.5O2/SiOx/Si (MIFIS) Gate Structure
- Publication Year :
- 2024
-
Abstract
- We study the impact of top SiO2 interlayer thickness on the memory window (MW) of Si channel ferroelectric field-effect transistor (FeFET) with TiN/SiO2/Hf0.5Zr0.5O2/SiOx/Si (MIFIS) gate structure. We find that the MW increases with the increasing thickness of the top SiO2 interlayer, and such an increase exhibits a two-stage linear dependence. The physical origin is the presence of the different interfacial charges trapped at the top SiO2/Hf0.5Zr0.5O2 interface. Moreover, we investigate the dependence of endurance characteristics on initial MW. We find that the endurance characteristic degrades with increasing the initial MW. By inserting a 3.4 nm SiO2 dielectric interlayer between the gate metal TiN and the ferroelectric Hf0.5Zr0.5O2, we achieve a MW of 6.3 V and retention over 10 years. Our work is helpful in the device design of FeFET.<br />Comment: 6 pages, 12 figures. arXiv admin note: substantial text overlap with arXiv:2404.15825
- Subjects :
- Condensed Matter - Materials Science
Physics - Applied Physics
Subjects
Details
- Database :
- arXiv
- Publication Type :
- Report
- Accession number :
- edsarx.2406.15478
- Document Type :
- Working Paper