Abstract

In this study, bioleaching method was used for kaolin sample taken from Kale Maden A.Ş.(Çan/ Çanakkale). Acidithiobacillus ferrooxidans bacteria, used in bioleaching experiments, were obtained from Deutsche Sammlung von Mikroorganismen und Zellkulturen (DSMZ). The effect of solids ratio on iron removal from the kaolin sample was investigated. pH, bacteria quantity and Fe concentration were measured in the experiments. Dissolution rates of Fe decreased with increasing solids ratio. The best iron removal was obtained as 59.44% Fe2O3 at 1% solids ratio.<br />Bu çalışmada, Kale Maden A.Ş. (Çan/Çanakkale)’den temin edilen kaolen numunesine biyoliç yöntemi uygulanmıştır. Biyoliç deneylerinde Deutsche Sammlung von Mikroorganismen und Zellkulturen (DSMZ) kültür koleksiyonundan temin edilen Acidithiobacillus ferrooxidans kullanılmıştır. Deneysel çalışmalarda katı-sıvı oranının demir giderimi işlemi üzerindeki etkileri araştırılmıştır. Deneyler sırasında; pH, bakteri sayısı ve çözeltiye geçen Fe derişimi ölçülmüştür. Biyoliç deneylerinde katı oranı arttıkça demir giderimi düşmektedir. En iyi demir giderimi %1 katı oranında %59,44 olarak elde edilmiştir

Details

ISSN :
25647024 and 25872613
Database :
OpenAIRE
Journal :
Volume: 50, Issue: 4 39-43, Scientific Mining Journal
Accession number :
edsair.tubitakulakb..8e106f313d52e17d2c4c4efc3b31f5f9