Metal-insulator-metal (MIM) capacitors with TiN and high thickness of Al2O3 above 50 nm were fabricated to address high voltage (>30 V) and linear capacitor applications. Atomic layer deposition is used to deposit both TiN and Al2O3 to guarantee a good composition and thickness control. The impact of the deposition process and post-treatment condition on the MIM capacitor's breakdown voltage is studied and correlated with time of flight-secondary ion mass spectrometry (ToF-SIMS). Higher deposition temperature and thermal treatment of TiN and Al2O3 after deposition increase breakdown voltage and improve uniformity. ToF-SIMS demonstrates that Al2O3 higher deposition temperature or rapid thermal processing annealing reduce the diffusion of TiN in Al2O3 leading to thinner TiN/Al2O3 interface layers that influence breakdown voltage and uniformity.

Details

Language :
English
Database :
OpenAIRE
Accession number :
edsair.od.......610..37461ecdfb5e4ff77c04a695c037ec3e