Surface effects on the degradation mechanism of bioactive PDMS-SiO2- CaO-P2O5 hybrid materials intended for bone regeneration

Authors :
D.A. Sánchez-Téllez
Luis M. Rodríguez-Lorenzo
Aitana Tamayo
Juan Rubio
M.A. Mazo
Lucía Téllez-Jurado
Dirección General de Investigación Científica y Técnica, DGICT (España)
Rodíiguez-Lorenzo, Luis Maria
Rodíiguez-Lorenzo, Luis Maria [0000-0002-4816-1087]
Source :
Digital.CSIC. Repositorio Institucional del CSIC, instname
Publication Year :
2017
Publisher :
Elsevier, 2017.

Abstract

The purpose of this work is to study the dissolution mechanism of SiO2-based bioactive hybrid materials containing both CaO and P2O5 in their structures and to determine the influence of apatite crystallization over the surface features of the hybrids during degradation. Hybrid materials were synthesized using sol–gel method. Tetraethoxysilane (TEOS), hydroxyl terminated polydimethylsiloxane (PDMS), Ca(NO3)2·4H2O, and triethyl phosphate (TEP) were used as reactants. The degradation and bioactivity of the hybrid materials were tested by soaking the specimens into simulated body fluid (SBF). Raman spectroscopy, tensiometry and N2 adsorption/desorption curves were used to measure the changes during the degradation experiments. Several mathematical approaches have been taken to analyze the results. The growth of an apatite layer on the surface of SiO2-modified PDMS-P2O5-CaO hybrid materials occurs together with degradation of the silica-based matrix. The dissolution kinetics depends upon the composition of the material. It varies from a surface-driven mechanism in the case of low-P2O5 samples to a degradation path which fits into a Weibull type kinetic model, typical of matrix dissolution processes in materials enriched in P2O5. During degradation, the surface parameters, fractal constant and anisotropy of the pores were determined. The slight increase of the fractal constant in low-containing P2O5 materials suggests the formation of a homogeneous silica-like layer in the first stage of degradation, which also works as anchoring nucleus for subsequent apatite formation. In all the cases, the degradation leads to ink-bottle shaped pores, increasing their volume as degradation occurs, but keeping their neck shape.<br />This work was supported by SIP-IPN 20150064 Project (Mexico), DGICYT Project, MAT2014-51918-C2-1-R (Spain), Fundación General CSIC (Programa ComFuturo) (A. Tamayo). DA Sánchez – Téllez also acknowledges CONACYT for the scholarship given.

Details

Language :
English
Database :
OpenAIRE
Journal :
Digital.CSIC. Repositorio Institucional del CSIC, instname
Accession number :
edsair.doi.dedup.....88aa83c293592b602336d6d9a098eb6f