Fabrication of V-substituted (Bi, M)4Ti3O12 [M = lanthanoids] thin films by chemical solution deposition method
- Source :
- Scopus-Elsevier
-
Abstract
- Bismuth titanate (Bi4Ti3O12; BIT) -based ferroelectric materials are proposed from the view of the “Site-engineering”, where the Bi-site ions are substituted by lanthanoid ions (La3+ and Nd3+) and Ti-site ions by other ions with higher charge valence (V5+). In the present study, influences of vanadium (V) - substitution for (Bi,M)4Ti3O12 thin films [M = lanthanoid] on the ferroelectric properties are evaluated. V-substituted (Bi,M)4Ti3O12 films have been fabricated using a chemical solution deposition (CSD) technique on the (111)Pt/Ti/SiO2/(100)Si substrate. Remnant polarization of (Bi,La)4Ti3O12 and (Bi,Nd)4Ti3O12 films has been improved by the V-substitution independent of the coercive field. The processing temperature of BLT and BNT films could also be lowered by the V-substitution.
Details
- Database :
- OpenAIRE
- Journal :
- Scopus-Elsevier
- Accession number :
- edsair.doi.dedup.....59752d4c411481d905371e0957541d02