Back to Search Start Over

Growth of Bi-Pb-Sr-Ca-Cu-O Films by Organic Chemical Spray Pyrolysis Deposition

Authors :
Ernesto Castillo-Apodaca
Elvia Díaz-Valdés
C. Mejía-García
Gerardo Contreras-Puente
Publication Year :
2006
Publisher :
Trans Tech Publications Ltd., 2006.

Abstract

Bi-Pb-Sr-Ca-Cu-O films were deposited at 270-420°C by organic chemical spray pyrolysis deposition with triphenyl bismuth (TPB), Pb(tmhd)2, Sr(tmhd)2, Ca(tmhd)2 and Cu(tmhd)2 (tmhd: 2,2,6,6-tetramethyl-3,5-heptanedione). A factorial experimental design was applied in order to study the interaction between composition, deposition temperature, annealing time and annealing temperature and the effect in the formation of crystalline phases. Results of their structural and chemical characterization are presented.

Details

Database :
OpenAIRE
Accession number :
edsair.doi.dedup.....2241f1b10cde8783b48cc1940e501e80
Full Text :
https://doi.org/10.4028/3-908158-03-6.43