Initiation and Performance of a Coating for Countering Chromium Poisoning in a SOFC-stack

Authors :
Dustin Beeaff
Åsa Helen Persson
Jens Valdemar Thorvald Høgh
Peter Vang Hendriksen
Lars Pilgaard Mikkelsen
Karsten Agersted Nielsen
Source :
ECS Transactions. 7:2145-2154
Publication Year :
2007
Publisher :
The Electrochemical Society, 2007.

Abstract

Minimising transport of chromium from the metallic interconnect (e.g. of Crofer 22APU) in a planar solid oxide fuel cell to the fuel cell cathode is done by application of a coating between the two parts. The coating is applied by slurry coating, and taken through stack initialisation it transforms into a stable and densely grown barrier layer, which minimises both the evaporation of chromium from the interconnect surface and the electrical contact resistance between the interconnect and the cathode. Between comparable stack element tests with and without coatings at 750ºC, the degra-dation rate in terms of power density decreased from 6.5% per 1000h to very low levels (

Details

ISSN :
19386737 and 19385862
Volume :
7
Database :
OpenAIRE
Journal :
ECS Transactions
Accession number :
edsair.doi...........e1b97d423e1e30d04c8e00f3a4681f87
Full Text :
https://doi.org/10.1149/1.2729329