ChemInform Abstract: Fracture Toughness of Chemically Vapor-Deposited Diamond

Authors :
Michael D. Drory
James S. Speck
Clayton F. Gardinier
Source :
ChemInform. 23
Publication Year :
2010
Publisher :
Wiley, 2010.

Abstract

The fracture toughness of chemically vapor-deposited diamond is estimated by a Vickers indentation method. Freestanding diamond films of 400-μm thickness are produced with plasma-enhanced chemical vapor deposition and highly polished for indentation testing. Indentation testing was performed with a microhardness tester using a load range of 5 to 8 N. The average fracture toughness is estimated as 5.3 ± 1.3 MPA · m1/2.