Back to Search Start Over

Nickel oxide reduction under nonisothermal conditions

Authors :
O. M. Niazyan
S. L. Kharatyan
E. G. Grigor’yan
Source :
Kinetics and Catalysis. 48:773-777
Publication Year :
2007
Publisher :
Pleiades Publishing Ltd, 2007.

Abstract

The interaction of nickel(II) oxide with carbon, polyethylene, and polystyrene in the temperature range 20–1000°C has been investigated by thermal analysis. The interaction of NiO with carbon and polyethylene under these conditions results in complete nickel reduction. In the case of polystyrene, because of its low decomposition temperature, the reduction process is incomplete. As compared to reduction with polyethylene, reduction with carbon takes place at a much higher temperature (750 versus 370°C) and requires a higher activation energy (68 ± 3 versus 41 ± 1 kcal/mol).

Details

ISSN :
16083210 and 00231584
Volume :
48
Database :
OpenAIRE
Journal :
Kinetics and Catalysis
Accession number :
edsair.doi...........a952f2a714d9e2340f4ee05a2266a893
Full Text :
https://doi.org/10.1134/s0023158407060018