Back to Search
Start Over
Thermo-oxidative degradation of some elastomers with a high content of 3,4 isoprene units
- Source :
- Polymer Degradation and Stability. 80:397-402
- Publication Year :
- 2003
- Publisher :
- Elsevier BV, 2003.
-
Abstract
- New elastomers with high content of 3,4 isoprene units have been developed during the last decades in an attempt to ensure superior performances of the final products and the present study is devoted to the investigation of some peculiarities of their ageing behaviour. On thermo-oxidative degradation, 3,4 isoprene units are less affected in comparison to cis -1, 4 and trans -1, 4 isoprene units. The degradation process consists mainly in splitting of the main chains at temperatures of 80–100 °C while at higher temperatures (120–130 °C) branching becomes a significant modification and this reaction is enhanced for the polymers containing preponderantly 3,4 units. Such behaviour leads to the fact that the processability of polymers containing high amounts of 1,2 and 1,3 isoprene units is less affected by thermo-oxidative degradation in comparison with cis -1, 4-polyisoprene, which could be explained by the fact that large amounts of double bonds are not present in the backbone of macromolecules but in the pendent groups.
- Subjects :
- chemistry.chemical_classification
Materials science
Polymers and Plastics
Double bond
Oxidative degradation
Polymer
Condensed Matter Physics
Branching (polymer chemistry)
Elastomer
chemistry.chemical_compound
chemistry
Mechanics of Materials
Materials Chemistry
Organic chemistry
Degradation process
Isoprene
Macromolecule
Subjects
Details
- ISSN :
- 01413910
- Volume :
- 80
- Database :
- OpenAIRE
- Journal :
- Polymer Degradation and Stability
- Accession number :
- edsair.doi...........7b987be345e80410043365dcf1aef47f
- Full Text :
- https://doi.org/10.1016/s0141-3910(02)00369-5