Abstract
- 20 vol.% aluminum borate whisker (Al18B4O33w) reinforced AC4CH alloy composite was fabricated by squeeze casting method. The matrix is controlled its impurities, which make metal alloys, especially AC4CH alloy that is made by restraining 0.2% Iron and aluminum to make a matrix material. The perform of composite materials was made from Al18B4O33w with 5% regulated three kinds of inorganic binders, SiO2, Al2O3 and TiO2 sol, respectively and then sintered at 1373K. The composites were obtained by squeeze cast infiltration of the molten alloy to the perform. Then it was squeeze casting into the matrix. The status of adhesions of whisker perform was Observed by SEM. Micro-Vickers hardness and tensile properties at the room temperature were estimated. Al18B4O33w/ AC4CH composites containing TiO2 sol has excellent properties on tensile properties and microvickers hardness compared with the other composites without inorganic binder, containing SiO2 and Al2O3 sol inorganic binder.
- Subjects :
- Materials science
Mechanical Engineering
Alloy
chemistry.chemical_element
engineering.material
Matrix (chemical analysis)
Metal
chemistry
Mechanics of Materials
Whisker
Impurity
Aluminium
visual_art
Ultimate tensile strength
engineering
visual_art.visual_art_medium
General Materials Science
Composite material
Boron
Subjects
Details
- ISSN :
- 16629795
- Database :
- OpenAIRE
- Journal :
- Key Engineering Materials
- Accession number :
- edsair.doi...........76e86248e4ca5f1d37c61a8907097967
- Full Text :
- https://doi.org/10.4028/www.scientific.net/kem.297-300.489