Back to Search
Start Over
Variation in Properties of Chitosan Prepared at Different Alkali Concentrations from Squid Pen and Shrimp Shell
- Source :
- International Journal of Polymeric Materials. 59:286-291
- Publication Year :
- 2010
- Publisher :
- Informa UK Limited, 2010.
-
Abstract
- Chitin from squid pen (Loligo sp.) and kiddi shrimp shell (Parapenaeopsis stylifera) were treated at room temperature (30 ± 2°C) with four different concentrations of sodium hydroxide: 20, 30, 40, and 50% w/w. With 50% sodium hydroxide solution, within 108 h, the chitin from squid pen was deacetylated to give chitosan. But it required 126 h at 40% and 144 h at 30% concentration of sodium hydroxide. In the case of chitin from Parapenaeopsis stylifera, complete deacetylation took place after 120 h and 168 h at 50 and 40% concentrations of sodium hydroxide, respectively. But shrimp shell on treatment with 20 and 30% sodium hydroxide solutions and squid pen kept at 20% sodium hydroxide were not sufficiently deacetylated even after 480 h. Properties like degree of deacetylation, viscosity and molecular weight of the prepared chitosan samples were studied. Minimum alkali concentration required for the formation of chitosan at room temperature was found to be 30% for squid chitin and 40% for shrimp chitin. With ...
Details
- ISSN :
- 1563535X and 00914037
- Volume :
- 59
- Database :
- OpenAIRE
- Journal :
- International Journal of Polymeric Materials
- Accession number :
- edsair.doi...........652ac8a81f61879dde4c907ab12ff411
- Full Text :
- https://doi.org/10.1080/00914030903333039