Wet vibro-grinding of zircon with surfactants

Authors :
S. T. Balyuk
G. V. Kukolev
I. G. Orlova
Ts. E. Paper
E. D. Posokhova
E. D. Lisovaya
P. P. Arkhipov
N. T. Dyrda
Source :
Refractories. 18:355-360
Publication Year :
1977
Publisher :
Springer Science and Business Media LLC, 1977.

Abstract

An investigation was carried out of the effect of various surfactants added during the wet vibrogrinding of zircon on the degree of dispersion of the powder and on the sintering of specimens molded from the powders. When added in proportions up to 0.2% all surfactants tested (naphthenate soap, Asidol, titanium soap, GKZh-94, GKZh-10, triethanolamine, and sugar) helped to reduce the time required to grind the zircon to a given fineness from 15–20 to 4 h, i.e., by a factor of about 2.5–4.

Details

ISSN :
15739139 and 00343102
Volume :
18
Database :
OpenAIRE
Journal :
Refractories
Accession number :
edsair.doi...........4b0ead900b09dec0087e29a2b672364d
Full Text :
https://doi.org/10.1007/bf01294098