Abstract

The use of waste materials in the concrete industry has been a topic of interest for researchers around the world in recent decades. In this research, the fracture toughness (Kc) of edge-notched disc bend (ENDB) specimens of self-compacting mortars containing 0%, 20%, 40%, 60%, 80% and 100% waste glass aggregates (WG) under the pure mode 1, mixed mode 1/3, mixed mode 3/1, and pure mode 3 in ages of 14, 28 and 56 days have been studied. The results show that the use of 20% and 40% of WG will improve the fracture toughness of the mortars. On the other hand, increasing the curing age from 14 to 28 days, with and without WG, improves the fracture toughness of samples significantly. Increasing the curing age has the highest impact on the results of pure mode 3. In addition, due to the effective fracture toughness results, pure mode 3 is introduced as critical loading condition for self-compacting mortars containing WG.

Details

ISSN :
09500618
Volume :
282
Database :
OpenAIRE
Journal :
Construction and Building Materials
Accession number :
edsair.doi...........230870f5b303a5197861847f26534cb1
Full Text :
https://doi.org/10.1016/j.conbuildmat.2021.122711