Abstract

GH4169 at 650 °C in atmosphere was investigated by using single edge notch tensile specimens. The number of main cracks and crack initiation mechanisms at the notch surface strongly depended on the grain size. The crack initiation life accounted for more percentages of the total fatigue life for the alloy with smaller grain size. The fatigue life generally increased with increasing crack initiation life. The small crack transited to long crack when its length reached ˜10 times the grain size.

Details

ISSN :
10050302
Volume :
35
Database :
OpenAIRE
Journal :
Journal of Materials Science & Technology
Accession number :
edsair.doi...........1ec1be049155e6096f4c035e6106aa69