Selective reduction separation and recovery of tellurium and bismuth from acidic leaching solution
- Source :
- Transactions of Nonferrous Metals Society of China; February 2023, Vol. 33 Issue: 2 p596-608, 13p
- Publication Year :
- 2023
-
Abstract
- A simple and efficient method was proposed to selectively separate and recover tellurium and bismuth in an acidic leaching solution of tellurium−bismuth ore by Na2SO3and Fe powder. Then, the selective reduction mechanism was investigated by SEM−EDS, XRD, XPS, ICP-OES, etc. 99.83% Te in leaching solution can be reduced by Na2SO3with an excess coefficient of 16 at 80 °C for 10 min, and the grade of crude tellurium can reach 93.78%. Besides, the stirring action can accelerate the reduction of Te because the dissolution of Na2SO3is promoted. Subsequently, 99.39% Bi in the reduced solution can be displaced by Fe powder with an excess coefficient of 7.5 at 60 °C for 40 min, and the grade of crude bismuth can reach 92.35%. Finally, cyclic leaching of tellurium−bismuth ore was adopted to enrich Te(IV) and Bi(III) concentrations and decrease the Fe(III) concentration in leaching solution, which can efficiently decrease the consumption of Na2SO3.
Details
- Language :
- English
- ISSN :
- 10036326
- Volume :
- 33
- Issue :
- 2
- Database :
- Supplemental Index
- Journal :
- Transactions of Nonferrous Metals Society of China
- Publication Type :
- Periodical
- Accession number :
- ejs62564479
- Full Text :
- https://doi.org/10.1016/S1003-6326(22)66131-4