Crystallization behavior and magnetic properties of the low rare-earth content (Nd=6 at. %) Nd–Fe–Co–V–B nanocomposite magnet ribbons prepared by rapid quenching method.
MLA
Ono, H., et al. “Crystallization Behavior and Magnetic Properties of the Low Rare-Earth Content (Nd=6 at. %) Nd–Fe–Co–V–B Nanocomposite Magnet Ribbons Prepared by Rapid Quenching Method.” Journal of Applied Physics, vol. 93, no. 10, May 2003, p. 8113. EBSCOhost, https://doi.org/10.1063/1.1538179.
APA
Ono, H., Tayu, T., Waki, N., Sugiyama, T., Shimada, M., Kanou, M., Yamamoto, H., & Takasugi, K. (2003). Crystallization behavior and magnetic properties of the low rare-earth content (Nd=6 at. %) Nd–Fe–Co–V–B nanocomposite magnet ribbons prepared by rapid quenching method. Journal of Applied Physics, 93(10), 8113. https://doi.org/10.1063/1.1538179
Chicago
Ono, H., T. Tayu, N. Waki, T. Sugiyama, M. Shimada, M. Kanou, H. Yamamoto, and K. Takasugi. 2003. “Crystallization Behavior and Magnetic Properties of the Low Rare-Earth Content (Nd=6 at. %) Nd–Fe–Co–V–B Nanocomposite Magnet Ribbons Prepared by Rapid Quenching Method.” Journal of Applied Physics 93 (10): 8113. doi:10.1063/1.1538179.