Abstract

This paper reports the pressureless sintering behavior and the activation energy of the powdered MAX phases Ti<subscript>3</subscript>SiC<subscript>2</subscript> and Ti<subscript>2</subscript>AlC. A non-isothermal technique was used to determine the sintering kinetic parameter. The Ti<subscript>3</subscript>SiC<subscript>2</subscript> and Ti<subscript>2</subscript>AlC MAX phases showed the maximum sintering rate at 1723 K, 0.14 and 0.10 µm/s, respectively. The sintering rate of the sample at different temperatures followed a cubic equation which was determined. The sintering activation energy (E<subscript>a</subscript>) for the Ti<subscript>3</subscript>SiC<subscript>2</subscript> and Ti<subscript>2</subscript>AlC samples was 362.1 kJ/mol and 640.3 kJ/mol, respectively. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
27307727
Volume :
4
Issue :
1
Database :
Complementary Index
Journal :
Discover Materials
Publication Type :
Academic Journal
Accession number :
178483410
Full Text :
https://doi.org/10.1007/s43939-024-00098-2