Fabrication of a Porous Low Refractive Index Anti-Reflective Coating with High Transmittance by Using the Porogen of Laureth-5 Carboxylic Acid.
- Source :
- Coatings (2079-6412); Apr2024, Vol. 14 Issue 4, p440, 9p
- Publication Year :
- 2024
-
Abstract
- A porous anti-reflective coating (P-ARC) with average transmittance in the visible range of 97.9% was fabricated through the sol-gel method, followed by calcination at a relatively low temperature (220 °C) using the porogen of Laureth-5 carboxylic acid via a one-step approach. The results demonstrated the coating had an absolute value that was 7.5% higher than that of bare glass (92%). The prepared porous anti-reflective coating had a refractive index as low as 1.21. The coating remained undamaged during 3M tape stripping tests while maintaining excellent light transmittance. This work presents a film that has good thermal stability, chemical stability, and mechanical stability. [ABSTRACT FROM AUTHOR]
Details
- Language :
- English
- ISSN :
- 20796412
- Volume :
- 14
- Issue :
- 4
- Database :
- Complementary Index
- Journal :
- Coatings (2079-6412)
- Publication Type :
- Academic Journal
- Accession number :
- 176906062
- Full Text :
- https://doi.org/10.3390/coatings14040440