Back to Search Start Over

Interface Welding via Thermal Pulse Sintering to Enable 4.6 V Solid‐State Batteries.

Authors :
Yao, Xiangming
Chen, Shiming
Wang, Changhong
Chen, Taowen
Li, Jiangxiao
Xue, Shida
Deng, Zhikang
Zhao, Wenguang
Nan, Bowen
Zhao, Yiqian
Yang, Kai
Song, Yongli
Pan, Feng
Yang, Luyi
Sun, Xueliang
Source :
Advanced Energy Materials; 3/8/2024, Vol. 14 Issue 10, p1-10, 10p
Publication Year :
2024

Abstract

NASICON‐type Li1.3Al0.3Ti1.7(PO4)3 (LATP) is one of the most promising solid‐state electrolytes (SSEs) to achieve high‐energy‐density solid‐state batteries (SSBs) due to its high ionic conductivity, high‐voltage stability, and low cost. However, its practical application is constrained by inadequate interfacial compatibility with cathode materials and significant incompatibility with lithium metal. In this work, a cost‐effective interface welding approach is reported, utilizing an innovative thermal pulse sintering (TPS) to fabricate LATP‐based solid‐state batteries. Initially, the rapid thermal pulses enhance the ionic conductivity of LATP SSE by inducing selective growth of LATP nanowires, effectively occupying interparticle voids. Additionally, this process results in the formation of a dense layer (GCM) comprising graphene oxide, carbon nanotubes, and MXene with a controlled Li+ transport pathway, facilitating lithium stripping and plating processes. Moreover, these thermal pulses facilitate the interfacial fusion between LATP and cathode materials, while avoiding undesired phase diffusion. As a result, SSBs with a LiCoO2 cathode deliver favorable cycle stability at 4.6 V, marking significant progress. This facile interface welding strategy represents a substantial step toward high‐energy‐density SSB development. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
16146832
Volume :
14
Issue :
10
Database :
Complementary Index
Journal :
Advanced Energy Materials
Publication Type :
Academic Journal
Accession number :
175918885
Full Text :
https://doi.org/10.1002/aenm.202303422