Cite
Steady-state interface construction of high-voltage nickel-rich lithium-ion battery cathodes by low-content LixCoO2 surface modification engineering.
MLA
Ye, Xiaolin, et al. “Steady-State Interface Construction of High-Voltage Nickel-Rich Lithium-Ion Battery Cathodes by Low-Content LixCoO2 Surface Modification Engineering.” Ionics, vol. 29, no. 8, Aug. 2023, pp. 3039–53. EBSCOhost, https://doi.org/10.1007/s11581-023-05056-1.
APA
Ye, X., Wei, J., Qiao, X., Ji, Y., & Chen, B. (2023). Steady-state interface construction of high-voltage nickel-rich lithium-ion battery cathodes by low-content LixCoO2 surface modification engineering. Ionics, 29(8), 3039–3053. https://doi.org/10.1007/s11581-023-05056-1
Chicago
Ye, Xiaolin, Jian Wei, Xinyu Qiao, Yuxuan Ji, and Bing Chen. 2023. “Steady-State Interface Construction of High-Voltage Nickel-Rich Lithium-Ion Battery Cathodes by Low-Content LixCoO2 Surface Modification Engineering.” Ionics 29 (8): 3039–53. doi:10.1007/s11581-023-05056-1.