One of the most important indicators of casting quality is porosity. The formation of pores is largely conditioned by the presence of hydrogen in the batch and subsequently in the melt. The gasification of the melt is the primary factor increasing the porosity of casts. This paper addresses the issue of reducing the melt gasification by using FDU (Foundry Degassing Unit) unit. The gas content in the melt is evaluated by determining the Dichte Index depending on the geometry and the degree of the FDU unit rotor wear. For experiments performed under the operating conditions, three types of graphite rotors with different geometries are used. The extent of melt gasification and the Dichte Index are monitored during the rotor wear, at a rate of 0%, 25%, 50%, 75% and 100% rotor wear. Secondly, the chemical composition of the melt is monitored depending on the design and wear of the rotor. It is proven that the design and the degree of rotor wear do not have significant effect on the chemical composition of the melt and all evaluated samples fell within the prescribed quality in accordance with EN 1706. With regard to the overall comparison of the geometry and wear of individual rotor types, it has been proven that, in terms of efficiency, the individual rotors are mutually equivalent and meet the requirements for melt degassing throughout the service life. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
19961944
Volume :
15
Issue :
14
Database :
Complementary Index
Journal :
Materials (1996-1944)
Publication Type :
Academic Journal
Accession number :
158298173
Full Text :
https://doi.org/10.3390/ma15144924