The compaction of initial powders, the bending strength, and the microhardness of 21R sialon ceramics obtained by hot pressing have been studied experimentally. It is found that the Sm<subscript>2</subscript>O<subscript>3</subscript> sintering additive substantially reduces the annealing temperature and enhances the properties of the ceramics. The samples of 21R sialon ceramics without additives, which are prepared by annealing at 1950°C, have a density of 3.01 g/cm<superscript>3</superscript>, a bending strength of 240 ± 15 MPa, and a Vickers microhardness of 16.2 ± 0.4 GPa; the samples of 21R sialon ceramics with 2.5 wt % Sm<subscript>2</subscript>O<subscript>3</subscript>, which are annealed at 1750°C, are characterized by a density of 3.39 g/cm<superscript>3</superscript>, a bending strength of 315 ± 16 MPa, and a Vickers microhardness of 21.9 ± 0.2 GPa. It is shown that Sm<subscript>2</subscript>O<subscript>3</subscript> reacts with 21R sialon in the temperature range of 1600–1700°C to form the 27R sialon and SmAlO<subscript>3</subscript> impurity phases. In the samples annealed at 1750°C, the 27R sialon and Sm–sialon (Sm<subscript>3</subscript>Si<subscript>2.5</subscript>Al<subscript>3.5</subscript>O<subscript>12.5</subscript>N<subscript>1.5</subscript>) impurity phases are detected. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
00360236
Volume :
66
Issue :
8
Database :
Complementary Index
Journal :
Russian Journal of Inorganic Chemistry
Publication Type :
Academic Journal
Accession number :
152058324
Full Text :
https://doi.org/10.1134/S0036023621080143