- The paper examines the production of Si-modified biogenic hydroxyapatite ceramics. The introduction of methylsilicic acid hydrogel in amounts converted to 2 and 5 wt.% Si and subsequent sintering at 600°C increase the specific surface area by 10 times, from 6.1 to 59.8 m/g. The porosity of ceramics increases from 43.0 to 62.3% when the modifying addition reaches up to 5 wt.%, the compressive strength being equal to 27-33 MPa. The modifying addition also influences the structure and reduces the minimum grain size of the material from 0.65 to 0.1μm [ABSTRACT FROM AUTHOR]
- Subjects :
- HYDROXYAPATITE
CERAMICS
HYDROGELS
POROSITY
MICROSTRUCTURE
GRAIN size
Subjects
Details
- Language :
- English
- ISSN :
- 10681302
- Volume :
- 54
- Issue :
- 1/2
- Database :
- Complementary Index
- Journal :
- Powder Metallurgy & Metal Ceramics
- Publication Type :
- Academic Journal
- Accession number :
- 103286780
- Full Text :
- https://doi.org/10.1007/s11106-015-9681-z