Effects of posttreatment on the metal-ceramic bond properties of selective-laser-melted Co-Cr dental alloy-Part 2: Heat treatment after porcelain firing.
MLA
Zhou, Yanan, et al. “Effects of Posttreatment on the Metal-Ceramic Bond Properties of Selective-Laser-Melted Co-Cr Dental Alloy-Part 2: Heat Treatment after Porcelain Firing.” The Journal of Prosthetic Dentistry, vol. 133, no. 1, Jan. 2025, pp. 292–300. EBSCOhost, https://doi.org/10.1016/j.prosdent.2023.01.030.
APA
Zhou, Y., Dong, X., Li, N., & Yan, J. (2025). Effects of posttreatment on the metal-ceramic bond properties of selective-laser-melted Co-Cr dental alloy-Part 2: Heat treatment after porcelain firing. The Journal of Prosthetic Dentistry, 133(1), 292–300. https://doi.org/10.1016/j.prosdent.2023.01.030
Chicago
Zhou, Yanan, Xin Dong, Ning Li, and Jiazhen Yan. 2025. “Effects of Posttreatment on the Metal-Ceramic Bond Properties of Selective-Laser-Melted Co-Cr Dental Alloy-Part 2: Heat Treatment after Porcelain Firing.” The Journal of Prosthetic Dentistry 133 (1): 292–300. doi:10.1016/j.prosdent.2023.01.030.