Back to Search Start Over

Poly (amido amine) and nano-calcium phosphate bonding agent to remineralize tooth dentin in cyclic artificial saliva/lactic acid.

Authors :
Liang K
Weir MD
Reynolds MA
Zhou X
Li J
Xu HHK
Source :
Materials science & engineering. C, Materials for biological applications [Mater Sci Eng C Mater Biol Appl] 2017 Mar 01; Vol. 72, pp. 7-17. Date of Electronic Publication: 2016 Nov 09.
Publication Year :
2017

Abstract

The objectives of this study were to develop a novel method to remineralize dentin lesions, and investigate the remineralization effects of poly (amido amine) (PAMAM) dendrimer plus a bonding agent with nanoparticles of amorphous calcium phosphate (NACP) in a cyclic artificial saliva/lactic acid environment for the first time. Dentin lesions were produced via phosphoric acid. Four groups were tested: (1) dentin control, (2) dentin with PAMAM, (3) dentin with NACP bonding agent, and (4) dentin with PAMAM plus NACP bonding agent. Specimens were treated with cyclic artificial saliva/lactic acid. The remineralized dentin was examined using scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), hardness and attenuated total reflection Fourier transform infrared spectroscopy (ATR-FTIR). NACP bonding agent yielded a dentin shear bond strength similar to commercial controls (Prime & Bond NT, Dentsply; Scotchbond Multi-purpose, 3M) (p>0.1). Increasing NACP in bonding agent from 0 to 40% did not affect bond strength. NACP bonding agent neutralized the acid and released Ca ions with concentrations of 4 to 20mmol/L, and P ions of 2 to 9mmol/L. PAMAM or NACP bonding agent alone achieved slight remineralization. The PAMAM+NACP group achieved the greatest dentin remineralization p<0.05). At 20days, PAMAM+NACP increased the hardness of pre-demineralized dentin to reach the normal dentin hardness (p>0.1). In conclusion, superior remineralization of PAMAM+NACP bonding agent was demonstrated for the first time. PAMAM+NACP bonding agent induced dentin remineralization under acid challenge, when conventional remineralization methods such as PAMAM alone did not work well. The novel PAMAM+NACP bonding agent method is promising to improve the longevity of resin-dentin bonds, inhibit caries, and protect teeth.<br /> (Copyright © 2016 Elsevier B.V. All rights reserved.)

Details

Language :
English
ISSN :
1873-0191
Volume :
72
Database :
MEDLINE
Journal :
Materials science & engineering. C, Materials for biological applications
Publication Type :
Academic Journal
Accession number :
28024641
Full Text :
https://doi.org/10.1016/j.msec.2016.11.020