Effect of tempering temperature on the toughness of 9Cr–3W–3Co martensitic heat resistant steel.
- Source :
-
Materials & Design . Feb2014, Vol. 54, p874-879. 6p. - Publication Year :
- 2014
-
Abstract
- Highlights: [•] Toughness of 9Cr–3W–3Co steel increases with increasing tempering temperature. [•] Toughness is influenced by hardness of base metal and length of crack propagation path. [•] Hardness of base metal is influenced by dislocation density and degree of supersaturation of the interstitial atoms. [•] Length of crack propagation path is influenced by length of the large angle boundaries. [Copyright &y& Elsevier]