Back to Search Start Over

Synthesis and thermoelectric properties of Sr0.95La0.05TiO3−δ -TiO2 solid solutions

Authors :
Liu, J.
Wang, H.C.
Su, W.B.
Wang, C.L.
Zhang, J.L.
Mei, L.M.
Source :
Solid State Sciences. Jan2010, Vol. 12 Issue 1, p134-137. 4p.
Publication Year :
2010

Abstract

Abstract: Sr0.95La0.05TiO3−δ solid solutions, combined with 10mol% TiO2, were prepared at different temperatures. When sintered at a suitable temperature, the Seebeck coefficient presents the same behavior at high temperatures as that of Sr0.95La0.05TiO3−δ ceramic. Otherwise, the Seebeck coefficient would be smaller. After introducing TiO2, both of the thermal and electrical conductivity are reduced. The sample sintered at 1350°C exhibits the highest ZT of about 0.2, which slightly larger than that of Sr0.95La0.05TiO3−δ ceramic. [Copyright &y& Elsevier]

Details

Language :
English
ISSN :
12932558
Volume :
12
Issue :
1
Database :
Academic Search Index
Journal :
Solid State Sciences
Publication Type :
Academic Journal
Accession number :
47362197
Full Text :
https://doi.org/10.1016/j.solidstatesciences.2009.10.018