Back to Search Start Over

Preparation of Reduced Iron Powder from High-Phosphorus Iron Ore: A Pilot-Scale Rotary-Kiln Investigation.

Authors :
You, Jinxiang
Zhang, Shuhui
Wu, Shichao
Yan, Li
Huang, Wusheng
Rao, Mingjun
Source :
Mineral Processing & Extractive Metallurgy Review. Sep2024, Vol. 45 Issue 6, p644-653. 10p.
Publication Year :
2024

Abstract

Dephosphorization is essential for utilizing high-phosphorus iron ore (HPIO), and this work prepared reduced iron powder via reductive roasting in a semi-industrial rotary kiln follower by magnetic separation. Under the conditions, reductive temperature of 1150°C, duration time of 60 min, mass ratio of briquettes to pea coal of 1:1, the reduced iron powder with an iron grade of 93.21% and phosphorus content of 0.13% was obtained, of which the corresponding iron recovery is 82.68% and dephosphorization ratio is 89.87%. The limestone reacted with gangue to form calcium aluminum silicate, preventing the reduction of phosphorate and in turn the formation of ferrophosphorus. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
08827508
Volume :
45
Issue :
6
Database :
Academic Search Index
Journal :
Mineral Processing & Extractive Metallurgy Review
Publication Type :
Academic Journal
Accession number :
178971413
Full Text :
https://doi.org/10.1080/08827508.2023.2227326