Engineering Sb/Zn4(OH)6SO4·5H2O interfacial layer by in situ chemically reacting for stable Zn anode.

Authors :
Xu, Mingyang
Li, Jing
Wang, Liyuan
Wang, Zhitao
Wang, Mingyu
Li, Liangsheng
Cai, Xiaowu
Li, Linpo
Shangguan, Enbo
Source :
Journal of Colloid & Interface Science. Oct2024, Vol. 671, p742-750. 9p.
Publication Year :
2024

Abstract

The two-phase protection layers induce a reinforcement effect on the Zn anode. Specifically, Sb nanoparticles can act as nucleation sites to promote the uniform Zn deposition and homogenize the electric field around the Zn surface. While ZHS micrometer-size sheets possess sufficient electrolyte wettability, fasting ion transfer kinetics and anti-corrosion, and thus guaranteeing uniform ion flux and suppressing dendrite growth and side reactions. [Display omitted] Rechargeable aqueous zinc ion batteries with abundant resources and high safety have gained extensive attention in energy storage technology. However, the cycle stability is largely limited by notorious Zn dendrite growth and water-induced interfacial side reactions. Here, a uniform and robust protection layer consisting of metal antimony (Sb) nanoparticles and micrometer-size sheets Zn 4 (OH) 6 SO 4 ·5H 2 O (ZHS) is purposely designed to stabilize Zn anode via an in situ chemical reaction strategy. The two-phase protection layers (Sb/ZHS) induce a reinforcement effect on the Zn anode (Zn@Sb/ZHS). Specifically, Sb nanoparticles play the part of nucleation sites to facilitate uniform Zn plating and homogenize the electric field around the Zn surface. ZHS micrometer-size sheets possess sufficient electrolyte wettability, fast ion transfer kinetics, and anti-corrosion, thus guaranteeing uniform ion flux and inhibiting H 2 O decomposition. As expected, the symmetric Zn@Sb/ZHS//Zn@Sb/ZHS cells achieve a minimal voltage hysteresis and a reversible cycle of over 2000 h at 1 mA cm−2. By pairing with the MnO 2 cathode, the full cell exhibits a significantly improved stability (∼94.17 % initial capacity after 1500 cycles). This study provides a new strategy to design artificial protection layers. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
00219797
Volume :
671
Database :
Academic Search Index
Journal :
Journal of Colloid & Interface Science
Publication Type :
Academic Journal
Accession number :
177846445
Full Text :
https://doi.org/10.1016/j.jcis.2024.05.153