Sulfide Inclusion-Induced Micro-scaled Pitting Corrosion on Crankshaft Surface in Indoor Atmospheric Environment.
MLA
Dong, Xiaomeng, and Dequn Kong. “Sulfide Inclusion-Induced Micro-Scaled Pitting Corrosion on Crankshaft Surface in Indoor Atmospheric Environment.” Journal of Failure Analysis & Prevention, vol. 24, no. 2, Apr. 2024, pp. 700–07. EBSCOhost, https://doi.org/10.1007/s11668-024-01893-y.
APA
Dong, X., & Kong, D. (2024). Sulfide Inclusion-Induced Micro-scaled Pitting Corrosion on Crankshaft Surface in Indoor Atmospheric Environment. Journal of Failure Analysis & Prevention, 24(2), 700–707. https://doi.org/10.1007/s11668-024-01893-y