Rapid hardening response of ultra-hard Ti-6Al-2Sn-4Zr-6Mo alloy produced by laser powder bed fusion.
- Source :
-
Scripta Materialia . Mar2023, Vol. 226, pN.PAG-N.PAG. 1p. - Publication Year :
- 2023
-
Abstract
- Post heat treatment is essential for additively manufactured alloys to eliminate residual stress and in some cases further improve mechanical performance. This study systematically investigated the hardening response of a Ti-6Al-2Sn-4Zr-6Mo alloy processed by laser powder bed fusion (LPBF) to a one-step heat treatment. The results revealed significant hardening at both 500 °C and 650 °C. Most notably, an ultra-high peak-hardness of 563VHN was achieved within 5 mins of heat treatment at 650 °C due to a unique martensite-decomposed α+β microstructure consisting of alternating long β laths that are ∼5 nm thick and α laths that are ∼35 nm thick, and within the α laths are also short β laths that are ∼2 nm thick with an ∼11 nm inter-spacing. The influence of both types of β laths on the α lath thickness was established and related to the ultra-high hardness observed, which provides new insight for the design of new metastable LPBF-processed Ti alloys. [Display omitted] [ABSTRACT FROM AUTHOR]
- Subjects :
- *POWDERS
*LASERS
*RESIDUAL stresses
*TITANIUM alloys
*MARTENSITIC transformations
Subjects
Details
- Language :
- English
- ISSN :
- 13596462
- Volume :
- 226
- Database :
- Academic Search Index
- Journal :
- Scripta Materialia
- Publication Type :
- Academic Journal
- Accession number :
- 161302439
- Full Text :
- https://doi.org/10.1016/j.scriptamat.2022.115209