Synthesis and optical properties of nanostructured ZnS and heteronanostructures based on zinc and silver sulfides.

Authors :
Sadovnikov, Stanislav I.
Ishchenko, Aleksey V.
Weinstein, Ilya A.
Source :
Journal of Alloys & Compounds. Aug2020, Vol. 831, pN.PAG-N.PAG. 1p.
Publication Year :
2020

Abstract

ZnS nanopowders have been synthesized by chemical deposition from aqueous solutions of zinc nitrate and sodium sulfide in the presence of sodium citrate or Trilon B. Ag 2 S/ZnS heteronanostructures have been prepared by co-deposition of zinc and silver sulfides. The size of nanoparticles in the deposited powders has been estimated by X-ray diffraction and transmission electron microscopy. A change in the ratio between the concentrations of reagents in the reaction mixtures made it possible to obtain ZnS nanopowders with an average particle size of 2–10 nm. The size of the nanoparticles in the prepared heteronanostructures is 8–10 nm. The diffuse reflection spectra have been measured and the corresponding absorption spectra of nanostructured ZnS and Ag 2 S/ZnS heteronanostructures have been analyzed using Tauc plots. The optical band gap E g of the studied sulfide nanostructures has been estimated. A blue shift of the optical absorption edge and an increase in the E g values from 3.59 to 3.72 eV are observed with a decrease in the size of ZnS nanoparticles. An increase in the Ag 2 S content in Ag 2 S/ZnS heteronanostructures leads to a decrease in the optical band gap. Pulsed cathodoluminescence of nanostructured ZnS and Ag 2 S/ZnS heteronanostructures have been investigated. It is found that the maxima of the luminescence spectra of nanostructured zinc sulfide are located at about 450 nm. Prepared samples of nanostructured ZnS possess a very short decay time and thanks to this property the prepared ZnS nanostructures can be used as a material for scintillation detectors. Image 1 • ZnS and Ag 2 S/ZnS heteronanostructures are synthesized by chemical deposition. • Band gap of ZnS at decreasing particle of 10 to 2 nm varies from 3.6 to 3.7 eV. • Adding Ag 2 S to ZnS leads to much larger change of the band gap E g. • An increase in x for (ZnS)·(Ag 2 S) x from 0 to 0.1 reduces E g from 3.6 to 2.1 eV. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
09258388
Volume :
831
Database :
Academic Search Index
Journal :
Journal of Alloys & Compounds
Publication Type :
Academic Journal
Accession number :
142978378
Full Text :
https://doi.org/10.1016/j.jallcom.2020.154846