Laser solid forming additive manufacturing TiB2 reinforced 2024Al composite: Microstructure and mechanical properties.
- Source :
-
Materials Science & Engineering: A . Feb2019, Vol. 745, p319-325. 7p. - Publication Year :
- 2019
-
Abstract
- Abstract The 2024Al alloy and 3%TiB 2 reinforced 2024Al composite were fabricated using laser solid forming (LSF). Different from the LSF processed 2024Al with a large columnar grain and apparent preferential growth orientation, TiB 2 reinforced 2024Al composite presents texture-less structure, consisting of the dendrite and fine equiaxed structures. Some TiB 2 particles distribute within the Al matrix, others distribute along the grain boundaries and intertwine with the Al 2 Cu phase. The incorporation of TiB 2 gives rise to significant grain refinement, which is one of the important reasons for the improvement of mechanical properties. Moreover, the TiB 2 reinforced 2024Al sample exhibits 284 MPa high tensile strength, 163 MPa yield strength, 108.5HV microhardness, and 18.7% excellent elongation. [ABSTRACT FROM AUTHOR]
Details
- Language :
- English
- ISSN :
- 09215093
- Volume :
- 745
- Database :
- Academic Search Index
- Journal :
- Materials Science & Engineering: A
- Publication Type :
- Academic Journal
- Accession number :
- 134226762
- Full Text :
- https://doi.org/10.1016/j.msea.2018.12.072