A study on degradation of germanium coating on Kapton used for spacecraft sunshield application.

Authors :
Esther, A. Carmel Mary
Dey, Arjun
Sridhara, N.
Yougandar, B.
Bera, Parthasarathi
Anandan, Chinnasamy
Rangappa, Dinesh
Sharma, Anand Kumar
Source :
Surface & Interface Analysis: SIA. 12/15/2015, Vol. 47 Issue 13, p1155-1160. 6p.
Publication Year :
2015

Abstract

Sunshield membranes made of germanium‐coated black polyimide (GBP) or Kapton are often used on the reflector/transmitter antenna of satellites for thermal control applications. However, the germanium top layer is prone to degrade during ground storage and implementation. Hence, vacuum/inert gas‐sealed packaging is required for storing the membranes, followed by a staggered fabrication schedule as the shelf‐life of the GBP is identified as only ~6 months. In the present study, microstructural, thermo‐optical, and electrical properties along with X‐ray photoelectron spectroscopy (XPS) studies for evaluating oxidation states of the as‐received and degraded GBP films have been investigated thoroughly. The radio frequency (RF) loss behavior of both the films has also been studied for S band (2.5–3.5 GHz), Ku band (10.5–14.5 GHz), and Ka band (30–35 GHz). Copyright © 2015 John Wiley & Sons, Ltd. [ABSTRACT FROM AUTHOR]

Details

Language :
English
ISSN :
01422421
Volume :
47
Issue :
13
Database :
Academic Search Index
Journal :
Surface & Interface Analysis: SIA
Publication Type :
Academic Journal
Accession number :
111382230
Full Text :
https://doi.org/10.1002/sia.5867