1. Influence wt.% of SiC and Borax on the Mechanical Properties of AlSi-Mg-TiB-SiC Composite by the Method of Semi Solid Stir Casting.
- Author
-
Bhiftime, E. I., Guterres, Natalino F. D. S, Haryono, M. B., Sulardjaka, and Nugroho, Sri
- Subjects
- *
SILICON carbide , *BORAX , *MECHANICAL behavior of materials , *METALLIC composites , *MICROSTRUCTURE - Abstract
SiC particle reinforced metal matrix composites (MMCs) with solid semi stir casting method is becoming popular in recent application (automotive, aerospace). Stirring the semi solid condition is proven to enhance the bond between matrix and reinforcement. The purpose of this study is to investigate the effect of the SiC wt.% and the addition of borax on mechanical properties of composite AlSi-Mg-TiB-SiC and AlSi-Mg-TiB-SiC/Borax. Specimens was tested focusing on the density, porosity, tensile test, impact test microstructure and SEM. AlSi is used as a matrix reinforced by SiC with percentage variations (10, 15, 20 wt.%). Giving wt.% Borax which is the ratio of 1: 4 between wt.% SiC. The addition of 1.5% of TiB gives grain refinement. The use of semi-solid stir casting method is able to increase the absorption of SiC particles into a matrix AlSi evenly. The improved composite presented here can be used as a guideline to make a new composite. [ABSTRACT FROM AUTHOR]
- Published
- 2017
- Full Text
- View/download PDF