1. Characterization of self-cleaning glasses using Langmuir–Blodgett technique to control thickness of stearic acid multilayers Importance of spectral emission to define standard test
- Author
-
Peruchon, L., Puzenat, E., Girard-Egrot, A., Blumb, L., Herrmann, J. M., Guillard, C., Institut de recherches sur la catalyse et l'environnement de Lyon (IRCELYON), Université Claude Bernard Lyon 1 (UCBL), Université de Lyon-Université de Lyon-Centre National de la Recherche Scientifique (CNRS)-Institut de Chimie du CNRS (INC), Institut de Chimie et Biochimie Moléculaires et Supramoléculaires (ICBMS), Université de Lyon-Université de Lyon-Institut National des Sciences Appliquées de Lyon (INSA Lyon), and Université de Lyon-Institut National des Sciences Appliquées (INSA)-Institut National des Sciences Appliquées (INSA)-Institut de Chimie du CNRS (INC)-École Supérieure Chimie Physique Électronique de Lyon-Centre National de la Recherche Scientifique (CNRS)
- Subjects
"Photocatalytic degradation" ,"Self-cleaning glass" ,Self-cleaning glass ,Langmuir–Blodgett ,[CHIM.CATA]Chemical Sciences/Catalysis ,Fatty acid ,[SDE.ES]Environmental Sciences/Environmental and Society ,"Fatty acid" ,Irradiation wavelength ,"Stearic acid" ,[SDV.BBM.BC]Life Sciences [q-bio]/Biochemistry, Molecular Biology/Biochemistry [q-bio.BM] ,Photocatalytic degradation ,"Irradiation wavelength" ,Stearic acid ,"Langmuir–Blodgett" - Abstract
International audience; The photocatalytic properties of commercialized self-cleaning glasses have been evaluated by the degradation of stearic acid C17H35COOH (SA), selected as a model molecule representative of fatty dirt. The relative amount of SA has been determined by measuring the FTIR peak area in the range 2752 and 2992 cm−1 corresponding to the C–H stretching bands. In order to estimate the thickness of one layer, the deposit of SA has been performed using the Langmuir–Blodgett (LB) method, which allows obtaining organized monomolecular layers of amphiphilic organics on a substrate. The thickness of one SA layer, obtained by Langmuir–Blodgett deposition, has been correlated to the FTIR signal. The photocatalytic degradation of a SA layer of a controlled thickness was carried out in a double jacket Pyrex reactor equipped with a UV Philips HPK 125 lamp. The photocatalytic degradation rate of the SA layer with different thicknesses was determined. The SA degradation rate was investigated under UV-A and UV-B irradiations to determine the influence of the photon wavelength range on efficiency.
- Published
- 2008