1. Preparation of In0.5Sc1.5Mo3O12 nanofibers and its negative thermal expansion property.
- Author
-
Liu, Hongfei, Zhang, Hang, Huang, Feiyu, Zhu, Jun, Wang, Wei, Zeng, Xianghua, and Zhang, Zhiping
- Subjects
- *
THERMAL expansion , *THERMAL properties , *HEAT treatment , *X-ray diffraction , *NANOFIBERS , *HIGH temperatures - Abstract
Orthorhombic In 0.5 Sc 1.5 Mo 3 O 12 nanofibers were prepared by electrospinning followed by a heat treatment. The effects of post-annealing temperatures on the phase composition, microstructure and morphology were investigated by XRD, SEM, HRTEM and XPS. Negative thermal expansion (NTE) behaviors of the In 0.5 Sc 1.5 Mo 3 O 12 nanofibers were analyzed by high-temperature XRD. Results indicate that the as-prepared In 0.5 Sc 1.5 Mo 3 O 12 nanofibers show an amorphous structure with smooth and homogeneous shape. The average diameter of the as-prepared In 0.5 Sc 1.5 Mo 3 O 12 nanofibers is around 515 nm. Well crystallized orthorhombic In 0.5 Sc 1.5 Mo 3 O 12 nanofibers could be prepared after post-annealing at 550 °C for 2 h with an average diameter of about 192 nm. The crystallinity of In 0.5 Sc 1.5 Mo 3 O 12 nanofibers gradually improved with the increase of annealing temperature. However, too high post-annealing temperature leads to a damage of sample's fiber structure. The high-temperature XRD results reveal that In 0.5 Sc 1.5 Mo 3 O 12 nanofibers show an anisotropic NTE, and the coefficients of thermal expansion (CTEs) along a -axis and c -axis were −5.95 × 10−6 °C−1 and -3.54 × 10−6 °C−1, while the one along b -axis is 5.61 × 10−6 °C−1. The volumetric CTE of In 0.5 Sc 1.5 Mo 3 O 12 nanofibers is −3.90 × 10−6 °C−1 and the linear one is 1.3 × 10−6 °C−1 in 25–700 °C. [ABSTRACT FROM AUTHOR]
- Published
- 2023
- Full Text
- View/download PDF